MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Baystar™ B5845 High Density Polyethylene - Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Bimodal HDPE Blow Molding Resin

Characteristics:

  • Excellent stress cracking resistance
  • Excellent stiffness

Applications:

  • Household chemicals
  • Industrial chemicals
  • Industrial parts
  • Food packaging
  • Personal care packages

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Key Words: Excellent stress cracking resistance; Excellent stiffness
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.958 g/cc0.0346 lb/in³ASTM D-792
ESCR 100% Igepal® >= 800 hour>= 800 hourASTM D1693, B
ESCR 10% Igepal® >= 300 hour>= 300 hourASTM D1693, B
Melt Flow 0.45 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 31.0 MPa4500 psiASTM D-638
Elongation at Break 200 %200 %ASTM D-638
Flexural Modulus  0.931 GPa
@Strain 2 %
135 ksi
@Strain 2 %
ASTM D-790
 1.14 GPa
@Strain 1 %
165 ksi
@Strain 1 %
ASTM D-790
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 204 °C360 - 400 °FBlow Molding Stock Temperature
Melt Temperature 193 - 216 °C380 - 420 °FExtrusion
 
Descriptive Properties
processBlow Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HD 6305 Blow Molding Resin
Chevron Phillips Marlex® HXM TR-570 High Density Polyethylene
ExxonMobil HD 5705 High Density Polyethylene Resin
ExxonMobil HD 6307 Blow Molding Resin
NOVA Chemicals Sclair® 58A/58A-DE3 HDPE Blow Molding Resin

PBAYST813 / 130468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.