MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

TSRC Taipol® 0150L BR
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Polymerization System: Solution Polymerization

Catalyst: Ziegler Cobalt Type

Configuration: 96% cis minimum

Stabilizer: Non-staining

Characteristics: High linearity; Excellent abrasion resistance; Low heat build-up; Good low temperature properties; High resilience; Good extrusion properties; Low hysteresis

Application: Mainly for tires, hoses, footwear, belts, golf ball, bouncing ball and industrial goods.

Test Recipe
Taipol BR-0150 – 100
HAF black (IRB#9) - 60.00
ASTM Type 103 Petroleum Oil - 15.00
Zinc Oxide- 3.00
Stearic Acid - 2.00
TBBS - 0.90
Sulfur - 1.50
Total - 182.40

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.910 g/cc0.910 g/cc
Volatiles <= 0.50 %<= 0.50 %Polymer Properties; ASTM D-5668
Mooney Viscosity  38 - 48
@Temperature 100 °C
38 - 48
@Temperature 212 °F
ML1+4, Polymer Properties; ASTM D-1646
 <= 75
@Temperature 100 °C
<= 75
@Temperature 212 °F
ML1+4, Compound Properties; ASTM D-1646
Ash <= 0.20 %<= 0.20 %Polymer Properties; ASTM D-5667
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 12.7 MPa>= 1850 psiCure @ 35 min for 145?; ASTM D-412
Elongation at Break >= 300 %>= 300 %Cure @ 35 min for 145?; ASTM D-412
300% Modulus 7.85 - 11.8 MPa1140 - 1710 psiCure @ 25 min for 145?; ASTM D-412
 8.83 - 12.7 MPa1280 - 1850 psiCure @ 35 min for 145?; ASTM D-412
 8.83 - 12.7 MPa1280 - 1850 psiCure @ 50 min for 145?; ASTM D-412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTSRC015 / 306303

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.