MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hogen Duralloy H20TC 70 Tungsten Carbide/30 Copper PM Metal Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Refractory Metal; Tungsten Alloy

Material Notes: Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.

Typical Resistance Welding Applications: Extremely hard and wear resistant to meet the more demanding requirements of electrical upsetting and electro-forging.

Data provided by Hogen Industries.

Key Words: Hogen Industries Powder Metallurgy Metal Composite; Copper Alloys
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 12.3 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 32
Tensile Strength, Ultimate 586 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000570 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µm/m-°C
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 30 %
WC 70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Resistohm® 125 Resistant Alloys Iron-Chromium-Aluminium Alloys
AISI Type S5 Tool Steel, austenitized 855-870°C (1575-1600°F), oil quenched to 55 HRC
Aperam Resistohm® 145 Resistant Alloys Iron-Chromium-Aluminium Alloys
Beryllium I-70H, Optical Grade
Beryllium IP-70, Powder

NHOG19 / 17327

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.