MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Silberline L-2422-PA
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: L-2422PA is a small particle size, bright leafing aluminum pigment based on standard cornflake geometry. It is a cost effective pigment for producing strong metallic effects with good coverage in liquid flexographic and gravure ink systems. This grade is produced as a pigment paste carried in isopropyl alcohol, but is not treated to inhibit the aluminum-water gassing reaction. L-2422PA is not recommended for use in aqueous inks unless a careful evaluation of its stability in the final ink formulation produces acceptable results.

Applications: Printing Inks

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.47 g/cc
Volatiles 35 %
Particle Size 9.0 µm
 
Descriptive Properties
CategoryLeafing
SolventsIsopropyl Alcohol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silberline SparkleBrite™ 190NL-PA
Silberline EternaBrite® Premier 251-PA
Silberline EternaBrite® 601-PA
Overview of materials for Polyamide-Imide, Molded
Overview of materials for Nylon 6, Cast

ESIBER248 / 6003

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.