MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem HRJ-11995 Resin
Categories: Polymer; Thermoplastic

Material Notes: Product Description: HRJ-11995 is a cashew nutshell oil-modified phenolic novolac resin. It has been formulated to have a reduced residual phenol content of less than 1%.

Applications: HRJ-11995 is intended for use as a reinforcing agent in elastomer-based compounds. It typically is used in combination with a methylene donor such as hexamethylenetetramine, commonly known as hexa. HRJ-11995 is commonly used at levels up to 30 parts resin per 100 parts rubber. The higher resin levels will provide more hardness, with less flexibility, in vulcanized elastomer compounds. Hexa levels are typically about 7 parts hexa per 100 parts HRJ-11995.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.16 g/cc
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 95.0 - 110 °C
 
Descriptive Properties
AppearanceFlake
Content0.01-0.75%Phenol

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH396 / 315314

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.