Softell CA 7413 A is a reactor TPO (thermoplastic polyolefin) manufactured using the LyondellBasell’s proprietary Catalloy process technology. It is suitable for the extrusion, calendaring and extrusion blow molding of very soft film and sheet as well as for injection molded parts. Softell CA 7413 A exhibits outstanding low stiffness, excellent low hardness and very good impact resistance. Softell CA 7413 A shows high compatibility to fillers and flame retardant additives as well as to other polyolefins. The grade is available in natural pellet form. Applications: Automotive Flooring, Interior Automotive Applications, Polymer Modifier, Single Ply Roofing, Soft Profile & Sheets, Soft Touch Applications, TPO Foils and Skins.Information provided by LyondellBasell. |