DuBois Alu-Braze 960 Aluminum Brazing Salt
Categories:
Ceramic
;
Fluid
;
Quenchant
Material Notes:
This is the standard salt designed for low melting point, good fluidity, and good braze characteristics.
Information provided by Heatbath Corporation - Park Metallurgical.
Heatbath/Park has been acquired by DuBois Chemicals.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Thermal Properties
Metric
English
Comments
Melting Point
516
°C
960
°F
Maximum Service Temperature, Air
649
°C
1200
°F
Upper limit of working range
Minimum Service Temperature, Air
538
°C
1000
°F
Lower limit of working range
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
DuBois Alu-Braze 930 Aluminum Brazing Salt
DuBois Alu-Braze 860 Aluminum Brazing Salt
Overview of materials for PVC, Rigid Grade
Lucas-Milhaupt AL 718 Aluminum Brazing Filler Metal
Superior Flux Superior No. 20 Aluminum Brazing Flux
WHEATB70 / 76025
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.