MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 800°C, 30 min.
Categories: Metal; Nonferrous Metal; Titanium Alloy; Beta Titanium Alloy

Material Notes: Good ductility and fabrication properties, aging yields extremely high strengths, low density.

Applications: Areospace and missile applications, springs

5 other heat treatments of this alloy are in MatWeb.

Key Words: Ti-13-11-3; B120VCA; UNS R58010
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.82 g/cc0.174 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 318318Estimated from Rockwell C.
Hardness, Knoop 346346Estimated from Rockwell C.
Hardness, Rockwell C 3434
Hardness, Vickers 333333Estimated from Rockwell C.
Tensile Strength 792 MPa
@Temperature 316 °C
115000 psi
@Temperature 601 °F
Tensile Strength, Ultimate 950 MPa138000 psi
Tensile Strength, Yield 860 MPa125000 psi
Elongation at Break 18 %18 %
Tensile Modulus 99.0 GPa14400 ksi
Modulus of Rigidity 42.7 GPa6190 ksi
Compressive Yield Strength 900 MPa131000 psi
Compressive Modulus 105 GPa15200 ksi
Notched Tensile Strength 1170 MPa170000 psiKt (stress concentration factor) = 3.0
Ultimate Bearing Strength 1860 MPa270000 psie/D = 2
Bearing Yield Strength 1380 MPa200000 psie/D = 2
Poissons Ratio 0.300.30
Fatigue Strength  140 MPa
@# of Cycles 1.00e+7
20300 psi
@# of Cycles 1.00e+7
Kt (stress concentration factor) = 3.0
 200 MPa
@# of Cycles 1.00e+7
29000 psi
@# of Cycles 1.00e+7
stress ratio = -1.0
 340 MPa
@# of Cycles 1.00e+7
49300 psi
@# of Cycles 1.00e+7
Unnotched
 375 MPa
@# of Cycles 30000
54400 psi
@# of Cycles 30000
stress ratio = -1.0
Fracture Toughness 88.0 MPa-m½80.1 ksi-in½KIC
Shear Modulus 43.0 GPa6240 ksi
Shear Strength 660 MPa95700 psiUltimate shear strength
Charpy Impact 20.0 J14.8 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000140 ohm-cm0.000140 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.70 µm/m-°C
@Temperature 20.0 - 95.0 °C
5.39 µin/in-°F
@Temperature 68.0 - 203 °F
Specific Heat Capacity  0.545 J/g-°C
@Temperature 20.0 °C
0.130 BTU/lb-°F
@Temperature 68.0 °F
 0.833 J/g-°C
@Temperature 425 °C
0.199 BTU/lb-°F
@Temperature 797 °F
Thermal Conductivity 6.90 W/m-K47.9 BTU-in/hr-ft²-°F
Beta Transus 700 °C1290 °FCommercial grade; lower for grades with lower oxygen content
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 3.0 %3.0 %
Carbon, C <= 0.10 %<= 0.10 %
Chromium, Cr 11 %11 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.35 %<= 0.35 %
Nitrogen, N <= 0.080 %<= 0.080 %
Oxygen, O <= 0.20 %<= 0.20 %
Titanium, Ti 73 %73 %
Vanadium, V 13 %13 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 850°C (1560°F) + Aged 510°C 8 hr
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Aged 490°C
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) SolnTreat; Age 450°C
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Solution Treated
Titanium Ti-13V-11Cr-3Al (Ti-13-11-3) Aged 400°C

MTB314 / 14186

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.