MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sandvik Bioline Pt10Ir Wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik Bioline platinum iridium alloy Pt10Ir is a precious metal wire that combine excellent biocompatible properties with excellent radiopacity, moderate strength and good formability. This alloy can be provided in an annealed, stress relieved or cold-worked condition depending on the post processing requirements. For medical use, Sandvik delivers Pt10Ir wires with the highest surface finish (Medical class) in order to maximize the fatigue strength which is critical in implant devices such as lead wires for cochlear implants and implant electrodes. Stress relieved conditioned wire are also often required when straightness is critical to the application.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 21.5 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 44Annealed
 50Stress relieved
 55Cold worked
Tensile Strength, Ultimate >= 380 MPaAnnealed
 >= 586 MPaStress relieved
 >= 896 MPaCold worked
Elongation at Break 2.0 %Cold worked
 3.0 %Stress relieved
 20 %Annealed
Modulus of Elasticity 202 GPaannealed
 219 GPawork-hardened
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
Specific Heat Capacity 0.485 J/g-°C
Thermal Conductivity 14.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Iridium, Ir 10 %
Platinum, Pt 90 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pt-10% Ir Alloy, Hard
Latrobe MP35N® Alloy

NSANDV5202 / 199766

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.