MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Daikin POLYFLON™ PTFE M-17 Polytetrafluoroethylene Molding Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Daikin- Polyflon™ M-17 is a polytetrafluoroethylene virgin granular fine cut resin. This general purpose molding powder has been specifically designed for use in medium to large billet compression molding.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.15 - 2.17 g/cc2.15 - 2.17 g/ccASTM D 4894
Bulk Density >= 0.380 g/cc>= 0.0137 lb/in³ASTM D 4894
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 30.0 MPa>= 4350 psiASTM D 4894
Elongation at Break >= 300 %>= 300 %ASTM D 4894
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 80.0 kV/mm
@Thickness 0.100 mm
>= 2030 kV/in
@Thickness 0.00394 in
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.5 - 3.7 %2.5 - 3.7 %
 
Descriptive Properties
AppearanceWhite Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daikin POLYFLON™ PTFE M-12 Polytetrafluoroethylene Molding Powder
AGC FL1650 PTFE
Daikin POLYFLON M-392 PTFE Molding Powder, Free Flow
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow
Chemours Teflon® PTFE 7A Granular Molding Powder

PDAIJ9880 / 209951

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.