MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones SilGlaze II SCS2800 Silicone Glazing Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: SCS2800 SilGlaze II silicone glazing sealant is a one-part, neutral, fast cure, medium modulus silicone sealant that develops significant green strength in the early cure hours. SCS2800 SilGlaze II silicone glazing sealant may be an excellent candidate for use as a bedding seal in the construction of residential and commercial doors and windows as well as a general-purpose weather and glazing sealant in new or remedial applications. Performance features: Silicone Durability, Primerless Adhesion, Fast Green Strength, ±50% Movement Capacity. Application: Excellent Process ability, Easy Repairs. SCS2800 SilGlaze II sealant may be used as a perimeter weather seal for field glazing, window installation and general purpose sealing applications. The sealant may be used for in-shop window fabrication as a bedding bead or for cap, toe and heel head applications.

Colors: Translucent (SCS2801), White(SCS2802), Black(SCS2803), Gray/Aluminum(SCS2809), Blue White(SCS2892), Bronze(SCS2897), Beige(SCS2800.0349)

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatile Organic Compounds (VOC) Content 33 g/lUncured; WPSTM C1454
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 19ASTM D2240
Tensile Strength, Ultimate 1.57 MPaASTM D412
Elongation, Ultimate 483 %ASTM D412
Peel Strength 57.0 pli
@Temperature 23.9 °C,
Time 1.81e+6 sec
50% Relative Humidity.; ASTM C794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -55.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 23.0 °C
@Time 1.81e+6 sec
Cure as Tested at 50% RH
Cure Time 72.0 - 96.0 hourMost common bead sizes.
 24.0 hour
@Temperature 24.0 °C
1/4" deep section.
Tack-Free Time 30.0 min
@Temperature 22.2 °C
50% RH; ASTM C679
Working Life 6.00 - 12.0 min
 
Descriptive Properties
AppearancePaste
Consistency / Sag0.1” max.ASTM D2202
Joint Movement Capability+/- 50%ASTM C719.
Silicone Content (%)100Uncured
UV & Weathering ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9922 / 265732

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.