MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parson Adhesives PARFIX® 3411 Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PARFIX 3411 is high viscosity combined with high temperature resistance, and excellent resistance to peel and shock loads. It is specifically formulated to bond various Rubbers, Metals, Wood and Plastics for use in challenging environments.

Applications:

  • Ideal for bonding Rubbers, Metals and Plastics.
  • Ideal for Speaker Assemblies, Automotive Components, Electronics Parts, Computer Assemblies, Electrical Components, etc.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Brookfield Viscosity 5000 - 6000 cP5000 - 6000 cPRTV
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 6.00 MPa870 psiPVC; ASTM D1002
 7.03 MPa1020 psiPolycarbonate; ASTM D1002
 10.0 MPa1450 psiSBR Rubber; ASTM D1002
 12.0 MPa1740 psiNeoprene Rubber; ASTM D1002
 12.0 MPa1740 psiNitrile Rubber; ASTM D1002
 17.0 MPa2470 psiAluminum; ASTM D1002
 13.0 - 25.0 MPa1890 - 3630 psi
 24.0 MPa3480 psiSteel; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 0.984 kV/mm25.0 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FASTM D696
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 98.9 °C210 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 125 °C257 °FASTM E228
Flash Point >= 93.0 °C>= 199 °F
 
Processing PropertiesMetricEnglishComments
Cure Time <= 0.0830 min<= 0.00138 hourNeoprene Rubber, Fixture
 <= 0.0830 min<= 0.00138 hourNitrile Rubber, Fixture
 0.167 - 0.4167 min0.00278 - 0.006945 hourAluminum, Fixture
 0.250 - 0.4167 min0.00417 - 0.006945 hourSBR Rubber, Fixture
 0.250 - 0.670 min0.00417 - 0.0112 hourABS, Fixture
 0.167 - 0.830 min0.00278 - 0.0138 hourPhenolic Materials, Fixture
 0.250 - 0.830 min0.00417 - 0.0138 hourSteel, Fixture
 0.500 - 1.33 min0.00833 - 0.0222 hourPolycarbonate, Fixture
 1440 min24.0 hourFull
 
Descriptive Properties
AppearanceHigh Viscosity Liquid
CompositionRubber Toughened Ethyl Cyanoacryalte
Gap Filling0.6 mm
Initial Strength Retained (%)75Gasoline for 1000 hrs at 22°C
 80Gasoline for 500 hrs at 22°C
 85Isopropanol for 500 hrs at 22°C
 85Isopropanol for 1000 hrs at 22°C
 90Motor Oil for 500 hrs at 40°C
 90Motor Oil for 1000 hrs at 40°C
 90Mineral Spirit for 500 hrs at 22°C
 90Mineral Spirit for 1000 hrs at 22°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPARSN121 / 186564

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.