MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kazanorgsintez 107-31 Compositions of Conductive and Semi-Conductive Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Production Method: Based on high pressure polyethylene grade 10703-020 or based on cable compositions grades 107-09K, and 107-10K.

Application: Designed for production of special cables.

Information Provided by Kazanorgsintez

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.15 %
@Temperature 195 - 205 °C
<= 0.15 %
@Temperature 383 - 401 °F
Carbon Black Loading >= 18.5 %>= 18.5 %
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break >= 80 %>= 80 %
Tear Strength Test >= 6.86>= 6.86MPa
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 10000 ohm-cm<= 10000 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -60.0 °C-76.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKAZAN065 / 127384

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.