Glass Fiber 30% - Aramid Fiber 15% - PTFE 15% Comments: - Aramid Fiber
- Aramid Fiber
- PTFE Lubricated
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company. Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade. |