MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds Plasti-Paste® II Trowelable Plastic Paste
Categories: Polymer; Thermoplastic

Material Notes: Product Overview: New Plasti-Paste™ II is a two component fiber-filled resin that is designed for vertical surface application. This no-odor formulation is an improved version of our original Plasti-Paste™ formula, and the cured product is different in the following ways: 1. Plasti-Paste II is now phthalate free. 2. Cured plastic can be painted (original Plasti Paste™ can not) and 3. It is harder, more rigid with better heat resistance. Part A is a liquid and Part B is a paste. New Mix Ratio is 1A: 2B by volume (62A:100B by weight). Pot life is 10 minutes at room temperature depending on mass. Demold time (can be handled) is about 90 minutes at room temperature depending on mass. Full cure; 24 hours at room temperature. Cure time can be accelerated by applying heat. Mixed material holds a vertical surface without sagging and cures to a strong, durable and lightweight plastic. Liquid material can be pigmented with So-Strong™ color tints from Smooth-On. This plastic can be used for creating themed environments or special effects, used as a “mother mold” material to reinforce rubber molds and a variety of other applications. This plastic is also a powerful adhesive and can be used as a repair material for a variety of industrial applications. Cured plastic can be sanded, machined and painted with acrylic enamel paints.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccASTM D-1475
Linear Mold Shrinkage 0.0050 cm/cm0.0050 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7070ASTM D-2240
Tensile Strength, Ultimate 14.8 MPa2150 psiASTM D-638
Elongation at Break 1.14 %1.14 %ASTM D-638
Tensile Modulus 1.62 GPa235 ksiASTM D-638
Flexural Strength 26.5 MPa3840 psiASTM D-790
Flexural Modulus 1.40 GPa203 ksiASTM D-790
Compressive Strength 34.3 MPa4980 psiASTM D-695
Compressive Modulus 0.432 GPa62.7 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 55.0 °C131 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 min1.50 hourHandling Time
Pot Life 10.0 min10.0 minASTM D-2471
 
Descriptive Properties
ColorOff-White
Mix Ratio1A:2Bby volume
 62A:100Bby weight
Mixed ViscosityPaste
Specific Volume27.7[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN047 / 296748

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.