Description: Rubber modified polypropylene produced for automotive interior applications using Mytex® Technology. Specifically designed to achieve ductile performance at cold temperatures during air bag deployment. Key Applications: Air bag deployable pillar and airbag trim Information provided by Mytex Polymers |