MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Superwool® HT Pyro-Bloc® Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Modules comprise two sections in edge grain orientation. These are held in position with two stainless steel tubes mounted transversely through the modules and remote from the hot face. They are anchored to the furnace casing with the patented Pyro-Bloc® internal hardware.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.160 - 0.192 g/cc
Loss On Ignition >= 0.25 %after 2 hours heating @ 800°C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.290 BTU/lb-°F
@Temperature 588 °C
Thermal Conductivity 0.0700 W/m-K
@Temperature 200 °C
at 160kg/m3; ASTM C-201
 0.0700 W/m-K
@Temperature 200 °C
at 240kg/m3; ASTM C-201
 0.0700 W/m-K
@Temperature 200 °C
at 192kg/m3; ASTM C-201
 0.0800 W/m-K
@Temperature 260 °C
at 160kg/m3; ASTM C-201
 0.100 W/m-K
@Temperature 400 °C
at 240kg/m3; ASTM C-201
 0.120 W/m-K
@Temperature 400 °C
at 192kg/m3; ASTM C-201
 0.140 W/m-K
@Temperature 400 °C
at 160kg/m3; ASTM C-201
 0.150 W/m-K
@Temperature 600 °C
at 240kg/m3; ASTM C-201
 0.170 W/m-K
@Temperature 600 °C
at 192kg/m3; ASTM C-201
 0.190 W/m-K
@Temperature 538 °C
at 160kg/m3; ASTM C-201
 0.210 W/m-K
@Temperature 600 °C
at 160kg/m3; ASTM C-201
 0.220 W/m-K
@Temperature 800 °C
at 240kg/m3; ASTM C-201
 0.250 W/m-K
@Temperature 800 °C
at 192kg/m3; ASTM C-201
 0.290 W/m-K
@Temperature 1000 °C
at 240kg/m3; ASTM C-201
 0.300 W/m-K
@Temperature 800 °C
at 160kg/m3; ASTM C-201
 0.330 W/m-K
@Temperature 1000 °C
at 192kg/m3; ASTM C-201
 0.330 W/m-K
@Temperature 816 °C
at 160kg/m3; ASTM C-201
 0.390 W/m-K
@Temperature 1200 °C
at 240kg/m3; ASTM C-201
 0.400 W/m-K
@Temperature 1000 °C
at 160kg/m3; ASTM C-201
 0.440 W/m-K
@Temperature 1200 °C
at 192kg/m3; ASTM C-201
 0.520 W/m-K
@Temperature 1093 °C
at 160kg/m3; ASTM C-201
 0.540 W/m-K
@Temperature 1200 °C
at 160kg/m3; ASTM C-201
Maximum Service Temperature, Air <= 1204 °C
Shrinkage 0.20 %
@Treatment Temp. 1000 °C,
Time 360000 sec
isothermal heating
 0.50 %
@Treatment Temp. 1100 °C,
Time 360000 sec
isothermal heating
 0.80 %
@Treatment Temp. 1200 °C,
Time 360000 sec
isothermal heating
 
Component Elements PropertiesOriginal ValueComments
CaO+MgO 18 - 25 %after firing
Other >= 3.0 %after firing
SiO2 70 - 80 %after firing
 
Descriptive Properties
Classification Temperature (°C)1300
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6450 / 203234

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.