MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotchcast™ 2136 Potting Kit
Categories: Polymer; Thermoset

Material Notes: The 3M Scotchcast Potting Kit 2136 is designed to provide protection against corrosion and possible deteriorating effects of fresh swimming pool or fountain water and sunlight by reliably encapsulating the 8 AWG ground connection in a wet-niche shell as required by NEC when using rigid, non-metallic conduit in the installation of wet-niche underwater lighting fixtures. Scotch cast 2136 compound is UL Listed as a potting compound for swimming pool, fountain or spa equipment and is for use only where adhering to copper, copper alloy and stainless steel materials.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/ccPolyol [Part B]; ASTM D891
 1.018 g/ccASTM D891
 1.02 g/ccMixed; ASTM D891
 1.077 g/ccPrepolymer [Part A]; ASTM D891
Viscosity 770 cPPrepolymer [Part A]; 3M Method TM-173
 1694 cPPolyol [Part B]; 3M Method TM-173
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83ASTM D2240
Tensile Strength at Break 6.43 MPa20'/min; ASTM D412
Elongation at Break 418 %20'/min; ASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 318 kV/inafter 7 days 100°C; ASTM D149
 334 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -80.0 °C
 
Descriptive Properties
AppearanceBlackPolyol [Part B]
 BlackMixed
 Pale to ClearPrepolymer [Part A]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP270 Black Structural Adhesive

PMM35242 / 169989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.