MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Universal Wire Works 312 Stainless Steel Electrode
Categories: Metal; Ferrous Metal; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Universal 312 electrodes were originally designed for the welding of high tensile alloys to high temperature heat resisting alloys on turbine engines. However, based upon performance these electrodes have found wide acceptance for the welding of newly developed high yield steels and abrasion resisting steels. The 312 deposit is excellent for welding dissimilar steels because of the high crack resistance and the highest tensile and yield strengths of any of the stainless arc welding electrodes commonly in use today.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Key Words: AWS E312-16
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 793 MPa115000 psi
Elongation at Break 23 %23 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.13 %0.13 %
Chromium, Cr 29 %29 %
Iron, Fe 59.9 %59.9 %As Remainder
Manganese, Mn 1.5 %1.5 %
Nickel, Ni 9.0 %9.0 %
Silicon, Si 0.50 %0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tantalum, UNS R05200
Superior Flux Superior No. 312 No-Clean Soldering Flux
MetalTek MTEK 29-10 Cast UNS J93403 Heat Resistant Stainless Steel
Universal Wire Works 29-9 (AMS 5784) Filler Metal
ATI AllvacĀ® NickelvacĀ® XM-19 UNS S20910 Specialty Steel

NUWW014 / 19593

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.