MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Network Polymers Kepital® F30-03
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Description: Natural Acetal Copolymer

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Moisture Absorption at Equilibrium 0.22 %23°C at 60% RH; ASTM D570
Linear Mold Shrinkage 0.020 cm/cmASTM D955
Melt Flow 27 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Procedure A Condition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ASTM D785
Tensile Strength at Break 9100 psiASTM D638
Elongation at Break 50 %ASTM D638
Tensile Modulus 418000 psiASTM D638
Flexural Strength 13300 psiASTM D790
Flexural Modulus 381000 psiASTM D790
Poissons Ratio 0.35
Shear Modulus 1.07 GPaCalculated
Shear Strength 8000 psiASTM D732
Izod Impact, Notched 1.00 ft-lb/inASTM D256
Izod Impact, Unnotched >= 20.0 ft-lb/inASTM D256
Coefficient of Friction 0.13Against Steel; Westover or Radial Type
 0.15Against Aluminum; Westover or Radial Type
 0.15Against Brass; Westover or Radial Type
 0.20Against Kepital; Westover or Radial Type
Taber Abrasion, mg/1000 Cycles 141 kg CS17 wheel; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dielectric Constant 3.7
@Frequency 100 Hz
ASTM D150
 3.7
@Frequency 1e+7 Hz
ASTM D150
Dissipation Factor 0.0010
@Frequency 100 Hz
ASTM D150
 0.0070
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 200 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Melting Point 329 °F10°C/min heating; DSC
Deflection Temperature at 0.46 MPa (66 psi) 158 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 230 °FASTM D648
Vicat Softening Point 162 °C0.125 inch bar, 1 Kg; ASTM D1525
Flammability, UL94 HB
@Thickness 0.0790 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Network Polymers Kepital® F20-03
KEP Kepital® F30-03 Acetal Copolymer, Low viscosity
Mitsubishi Iupital® F30-03 Copolymer Acetal
BASF Ultramid® B3GK24 BK 00564 10/20% Glass/Glass Bead Filled PA6 (Dry)
Network Polymers Kepital® F40-03

PDIAM155 / 29993

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.