MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Quadrant Symalit® 1000 ETFE unfilled, lining industries (ISO Data)  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Fluorocarbon ETFE/ECTFE, Molded/Extruded

Material Notes:
  • Service temperature range from -190 °C up to +155 °C / -310 °F up to +311 °F
  • Mechanical and technical features correspond to those of ECTFE
  • Excellent weather proof and radiation proof
  • Low water adsorption
  • Excellent resistance of abrasion

In January 2016 the Symalit® Fluoroplastics production assets were sold to AGRU Kunststofftechnik GmbH

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 155 °C311 °F
Minimum Service Temperature, Air -190 °C-310 °F
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) UnacceptableUnacceptable
Alkalies, Weak LimitedLimited
Chlorinated Solvents LimitedLimited
Continuous Sunlight LimitedLimited
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Modified ETFE, Unreinforced
Quadrant Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data)
Quadrant Symalit® ECTFE Ethylene-Chlorotrifluoroethylene (ASTM Product Data Sheet)
3M Dyneon™ ET 6235Z Fluorothermoplastic Granules
AGC Fluon® LM-720AP LM-ETFE Fluororesin

PQUADU918 / 130699

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.