MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RJM International TPS-G 85A TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information provided by RJM International

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Tensile Strength 9.32 MPa1350 psiASTM D412
 6.52 MPa
@Temperature 63.0 °C,
Time 1.80e+6 sec
946 psi
@Temperature 145 °F,
Time 500 hour
Weather Resistance; W-O-M
 8.292 MPa
@Temperature 136 °C,
Time 605000 sec
1203 psi
@Temperature 277 °F,
Time 168 hour
Heat Aging; ASTM D573
Elongation at Break 500 %500 %ASTM D412
 375 %
@Temperature 63.0 °C,
Time 1.80e+6 sec
375 %
@Temperature 145 °F,
Time 500 hour
Weather Resistance; W-O-M
 425 %
@Temperature 136 °C,
Time 605000 sec
425 %
@Temperature 277 °F,
Time 168 hour
Heat Aging; ASTM D573
Tear Strength 49.0 kN/m280 pliASTM D624 Die C
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -45.0 °C-49.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 210 °C338 - 410 °FInjection
 
Descriptive Properties
ColorNatural or Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRJMI039 / 296507

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.