MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reliance Industries Repol H110MS Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: REPOL Polypropylene H110MS is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H110MS is recommended for injection molding processes. Repol H110MS is an ideal choice for molding furnitures. It is also suitable for applications where high stiffness is desired. Repol H110MS contains antistat agent that reduces static charge build-up on products.

Features:

  • High stiffness
  • Low static charge buildup and reduced dust pickup
  • Consistent processability
  • Excellent color and processing stability
  • Information provided by Reliance Industries

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Melt Flow 11 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Yield 36.0 MPa50mm/min; ASTM D638
    Elongation at Yield 10 %50mm/min; ASTM D638
    Flexural Modulus, 1% Secant 1.75 GPaASTM D790A
    Izod Impact, Notched 35.0 J/m
    @Temperature 23.0 °C
    ASTM D256
     
    Thermal PropertiesOriginal ValueComments
    Deflection Temperature at 0.46 MPa (66 psi) 120 °CASTM D648

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Reliance Industries Polypropylene Random Copolymer
    Reliance Industries Repol H080EG Polypropylene
    Reliance Industries Repol H110MA Polypropylene
    Reliance Industries Repol H080EY Polypropylene
    Reliance Industries Repol H100EY Polypropylene

    PREL047 / 65387

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.