MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Aptek 1301 B/C/B Thermally conductive urethane film adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: Thermally conductive, electrically insulating hybrid urethane film adhesive
APTEK 1303B/C/B is a low modulus, flexible, void free, electrically insulating hybrid urethane film adhesive designed to bond dissimilar components and substrates. This B/C/B system is designed to manage stresses developed from mismatches of thermal expansion coefficients during temperature cycling as well as to dissipate heat generated from components and circuitry. APTEK 1303 B/C/B technology incorporates a partially-cured (B-staged) adhesive on both faces of a fully-cured (C-staged) ultra low modulus film. APTEK 1303 B/C/B film is a 100% solids, thermoset polymer, which will not outgas, while in place and is suitable for high vacuum environments. The film exhibits outstanding reversion resistance and physical stability under long-term aging of high humidity and heat.

Low modulus/high elongation for minimum stress buildup under components; Low Tg-remains flexible to -75°C; Exceeds NASA outgassing requirements for high vacuum environments; Typical film thickness, .006" to .012". Customer thicknesses available; Available in sheet or die-cut forms; Low tack adhesive layer allows for easy placement and, if needed, repositioning on assemblies

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.82 g/ccASTM D1475
Moisture Absorption at Equilibrium 0.15 %Cured property; ASTM D570
Outgassing - Total Mass Loss 0.45 %Cured property; at 10E-6 torr; ASTM E595
Collected Volatile Condensable Material 0.030 %Cured property; at 10E-6 torr; ASTM E-595
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 70 %
@Thickness 0.203 mm
Cured; ASTM D638
Tensile Modulus 750 psiASTM D638
 600 psi
@Temperature 55.0 °C
ASTM D638
Shear Strength 500 psiAl to Al, 10 mil bondline; ASTM D1002
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+14 ohm-cmCured property; ASTM D257
Dielectric Constant 5.8
@Frequency 1000 Hz
Cured property; ASTM D150
Dielectric Strength >= 1000 V/mil
@Thickness 0.127 mm
Cured; ASTM D149
Dissipation Factor 0.030
@Frequency 1000 Hz
Cured property; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 1; ASTM E831-86
 160 µm/m-°C
@Temperature 20.0 °C
Cured property; alpha 2; ASTM E831-86
Thermal Conductivity >= 1.50 W/m-K
Glass Transition Temp, Tg -75.0 °CCured property; ASTM E831-86
 
Processing PropertiesOriginal ValueComments
Processing Temperature 125 °CCure 1 hrs
Shelf Life 4.00 Month
@Temperature -40.0 °C
JMTP C-100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Liquid
Aptek 2201-A/B Fast set urethane adhesive
Abatron AboThane 8003-3 Polyurethane Coating
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound

PAPTEK23 / 24185

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.