MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon 55173R045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Silicone, Molded, Glass Fiber Filled

Material Notes: Design/Construction:
Interleave: Polyethylene
Layer 2: Cured Silicone Rubber
Substrate: Style 162 Fiberglass
Layer 1: Cured Silicone Rubber

Product Use: Press Pad

Appearance: Red silicone rubber on fiberglass cloth

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³Silicone Property; Arlon SQA-TMS-024
Thickness 74.9 microns2.95 milInterleave
 330 microns13.0 milSide 1; Arlon SQA-TMS-003
 330 microns13.0 milSide 2; Arlon SQA-TMS-003
 478 microns18.8 milSubstrate; Arlon SQA-TMS-003
 1140 microns45.0 milOverall; Arlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6161Silicone Property; ASTM D2240
 7575Product Property; ASTM D2240
Tensile Strength 8.07 MPa1170 psiSilicone Property; ASTM D412
Elongation at Break 682 %682 %Silicone Property; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 300 °C572 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 60.0 Month
@Temperature 23.0 °C
60.0 Month
@Temperature 73.4 °F
From date of manufacture
 
Descriptive Properties
ColorNaturally WhiteSubstrate
 Red
Total Product Weight (g/m2)1665Arlon SQA-TMS-025

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Chemfab® SlipGrip™ 10 PTFE/Silicone Coated Fiberglass Fabric
Haysite Thermalate® H330 Glass Mat Reinforced Polyester Laminate

PARL348 / 125534

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.