MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Primex Plastics Prime HMWPE 1000 SR High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Prime HMWPE 1000 SR is a co-extruded product consisting of a cap layer on both sides of the sheet to provide a skid resistant surface.

Applications: Prime HMWPE 1000 SR is designed for pallets, dunnage trays, truck bed liners or any other parts that require a high COF.

Information provided by Primex Plastics Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.946 g/cc0.946 g/ccASTM D1505
Environmental Stress Crack Resistance >= 600 hour>= 600 hourCond A, F50; ASTM D1693-79
Melt Flow 12 g/10 min12 g/10 minASTM D1238-89
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.7 MPa3000 psiASTM D638-89
Flexural Modulus 1.17 GPa170 ksiASTM D790
Izod Impact, Notched 2.67 J/cm5.00 ft-lb/inASTM D256 A
Coefficient of Friction 0.440.44ASTM D3028
 
Thermal PropertiesMetricEnglishComments
CTE, linear 126 µm/m-°C70.0 µin/in-°FASTM D696-79
Melting Point 130 °C266 °F
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °C140 °FASTM D648-82
Vicat Softening Point 116 °C240 °FASTM D1525-82

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRIM019 / 278490

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.