MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Envalior Durethan® ECO BV 35 H2 900500 Nylon 6, 35% Glass Fiber
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: PA 6, 35% glass fibers, injection molding, heat-ageing stabilized, contains 30% pre-consumer recycled material

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cm0.00050 - 0.0020 in/inPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in60x60x2; 290°C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inPost-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/in60x60x2; 290°C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 165 MPa23900 psid.a.m.; ISO 527-1, -2; 5 mm/min
Elongation at Break 3.0 %3.0 %d.a.m.; ISO 527-1, -2; 5 mm/min
Tensile Modulus 10.5 GPa1520 ksid.a.m.; ISO 527-1, -2; 1 mm/min
Flexural Strength 260 MPa
@Strain 3.5 %
37700 psi
@Strain 3.5 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Modulus 9.80 GPa1420 ksid.a.m., 2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  <= 10.0 kJ/m²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
cond.; ISO 180-1A
 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
d.a.m.; ISO 180-1A
Izod Impact, Unnotched (ISO)  60.0 kJ/m²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
d.a.m.; ISO 180-1U
 70.0 kJ/m²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
d.a.m.; ISO 180-1U
Charpy Impact Unnotched  6.00 J/cm²
@Temperature -30.0 °C
28.6 ft-lb/in²
@Temperature -22.0 °F
d.a.m.; ISO 179-1eU
 7.50 J/cm²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
d.a.m.; ISO 179-1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
d.a.m.; ISO 179-1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
d.a.m.; ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10°C/min; ISO 11357-1, -3
Deflection Temperature at 0.46 MPa (66 psi) 217 °C423 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 - 290 °C518 - 554 °F
 280 °C536 °Ffor test specimens; ISO 294
Mold Temperature 80.0 °C176 °Ffor test specimens; ISO 294
 80.0 - 120 °C176 - 248 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2 - 6 hour2 - 6 hour
Moisture Content 0.030 - 0.12 %0.030 - 0.12 %residual; Karl Fischer Test
 
Descriptive Properties
ISO Short NameISO 1874-PA 6, GHR, 14-100, GF35

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Durethan® TP 202-027 901510 Nylon 66 (PA66), 30% Glass/Carbon Fiber Reinforced, Dry

PLANX0650 / 133613

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.