Titanvene™ HD6070EA is a high density polyethylene copolymer with a narrow molecular weight distribution. It is suitable for a wide range of injection molding applications. Titanvene™ HD6070EA is characterized by easy processing, high rigidity, good impact resistance and high warpage resistance. Applications: Titanvene™ HD6070EA is designed for: Bottle crates. - Pails and containers; Pallets and structural foam. - Tube shoulder; Caps for still drinking water; Caps for non-carbonated beverages. Information provided by Lotte Advanced Materials. |