System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Syensqo (Solvay Specialty Polymers) Meforex® 123 Ozone-Friendly CFC Replacement
Categories:
Fluid
Material Notes:
Formula: CHCl
2
CF
3
; Name: 1,1 Dichloro 2,2,2 Trifluoroethane. Replaces CFC 11. Industrial air-conditioning, heat pumps, and heat transfer fluid.
Information provided by Solvay Solexis, Inc.
Key Words:
CHCl2CF3
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.46
g/cc
@Temperature 25.0 °C
0.0527
lb/in³
@Temperature 77.0 °F
Liquid
Molecular Weight
152.9
g/mol
152.9
g/mol
Vapor Pressure
0.910
bar
@Temperature 25.0 °C
683
torr
@Temperature 77.0 °F
Chemical Properties
Metric
English
Comments
Critical Pressure
36.68
bar
27510
torr
Critical Temperature
183.8
°C
362.8
°F
Critical Density
0.550
g/cc
0.0199
lb/in³
Thermal Properties
Metric
English
Comments
Heat of Vaporization
170
J/g
73.1
BTU/lb
at Boiling Point
Melting Point
-107.1
°C
-160.8
°F
at 1.013 bar
Boiling Point
27.8
°C
82.0
°F
at 1.013 bar
Descriptive Properties
Flammability Range (vol%)
None
Ozone Depletion Potential
0.022
Based on CFC11 = 1.0
Toxicity Level
1000 ppm
Allowed limit in work places, values suggested by AIHA (American Industrial Hygiene Association).
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
WAUSI09 / 74568
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.