MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

HB Fuller SIGEL Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: SIGEL is a high viscosity gel, surface insensitive cyanoacrylate adhesive that is used in applications that require faster cure speeds, on parts that are dry, and on parts that may be acidic. The SI Series bonds a wide range of similar and dissimilar surfaces. The SI Series provides exceptional performance in a wide range of applications.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Storage Temperature <= 22.0 °C<= 71.6 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 12.4 MPa>= 1800 psiISO 6922
Shear Strength >= 5.17 MPa>= 750 psiNeoprene; ISO 4587
 >= 5.86 MPa>= 850 psiPhenolic; ISO 4587
 >= 6.21 MPa>= 901 psiABS; ISO 4587
 >= 6.21 MPa>= 901 psiPVC; ISO 4587
 >= 6.21 MPa>= 901 psiPolycarbonate; ISO 4587
 >= 12.1 MPa>= 1750 psiAluminum; ISO 4587
 >= 14.5 MPa>= 2100 psiSteel; ISO 4587
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 - 1.00e+16 ohm-cm2.00e+15 - 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.0 - 3.5
@Frequency 1000 Hz
2.0 - 3.5
@Frequency 1000 Hz
ASTM D150
Dissipation Factor <= 0.020
@Frequency 1000 Hz
<= 0.020
@Frequency 1000 Hz
ASTM D150
 
Processing PropertiesMetricEnglishComments
Cure Time <= 0.0833 min<= 0.00139 hourSet Time: Neoprene
 <= 0.167 min<= 0.00278 hourSet Time: ABS
 <= 0.167 min<= 0.00278 hourSet Time: PVC
 <= 0.167 min<= 0.00278 hourSet Time: Polycarbonate
 <= 0.333 min<= 0.00556 hourSet Time: Steel
 <= 0.333 min<= 0.00556 hourSet Time: Aluminum
 
Descriptive Properties
Base compoundHigh Viscosity Gel
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL186 / 316977

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.