MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Materion WS185 Solder
Categories: Metal; Nonferrous Metal; Indium Alloy; Lead Alloy; Solder/Braze Alloy

Material Notes: Available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.

Former product of Williams Advanced Alloys. Williams Advanced Alloys is now a part of Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.52 g/cc0.308 lb/in³
 8.52 g/cc0.308 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 28.6 MPa4150 psi
Tensile Strength, Ultimate 28.6 MPa4150 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00002457 ohm-cm0.00002457 ohm-cm
 0.0000246 ohm-cm0.0000246 ohm-cm7% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear  27.0 µm/m-°C
@Temperature 20.0 °C
15.0 µin/in-°F
@Temperature 68.0 °F
 27.0 µm/m-°C
@Temperature 20.0 °C
15.0 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 29.0 W/m-K201 BTU-in/hr-ft²-°F
 29.0 W/m-K201 BTU-in/hr-ft²-°F
Melting Point 173 - 185 °C343 - 365 °F
Solidus 173 °C343 °F
Liquidus 185 °C365 °F
 
Component Elements PropertiesMetricEnglishComments
Indium, In 60 %60 %
Lead, Pb 40 %40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 204 In-Pb Solder Alloy
Indium Corp. Indalloy® 205 In-Pb Solder Alloy
Indium Corp. Indalloy® 231 Sn-Zn-In-Bi Solder Alloy
Cobalt Silicide, CoSi2
Chromium Silicide, CrSi2

NWILL45 / 19933

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.