MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Label-Lyte™ 28LLG MET OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A clear, one-side metallized, one-side treated oriented polypropylene film. The metalized layer is designed to provide a bright metal appearance in surface print or laminated applications. The treated, satin-white side is designed for machinability and hot melt adhesion. 28 LLG MET is designed for use in roll-fed labeling of cylindrical glass, plastic, and metal containers. Typical applications include food, beverage, nutritional, aerosol, and household chemicals. This film can be used as an inside web in lamination.

Availability: Latin America, North America and South America

Key Features:

  • Excellent opacity and bright metal background for outstanding graphic appeal
  • Very good hot melt adhesion
  • Consistent machinability on roll-fed label machines
Features:
  • Two Side Processable
Applications:
  • Beverage, Carbonated
  • Beverage, Mineral Waters
  • Dairy Products
  • Dry Foods and Beverage Powders
  • Health and Beauty Care
  • Household and Detergents
  • Industrial
Uses:
  • Reel-Fed Labels
Processing Method: Inner Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.10 milExxonMobil Method
Coating Weight 10.8 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 110 %20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Elongation at Break, TD 40 %20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Coefficient of Friction 0.36Adhesive Surface; ExxonMobil Method
 0.60Print Surface; ExxonMobil Method
Film Tensile Strength at Break, MD 10400 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 17400 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 5.0 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Optical Density 2.3ExxonMobil Method
 
Descriptive Properties
Wetting Tension0.85 receding cos thetaPrint Surface
Yield40000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Metallyte™ 100 MET OPP Film
ExxonMobil Label-Lyte® 350 LLG-MET Metallized, White Opaque OPP Film
ExxonMobil Label-Lyte® 260 LLG-MET Metallized, White Opaque OPP Film

PEX99548 / 175784

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.