The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use. Applications: - Bags for hosiery, shirts and other textiles.
- Food packaging for fresh fruits and produce.
Advantages: - Good optical properties.
- Excellent stiffness.
- High slip development and good open-ability.
Fabrication: - Equipment - general water quench blown film machines.
- Techniques - standard processing. Extrusion and water bath conditions can be varied to obtain the desired optical and mechanical film properties
Information provided by Titan Chemicals CAS# 9003-07-0 |