MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nylene® NX4569 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Dry as molded. Nylene NX4569 is a medium viscosity, molding grade nylon 6 resin suitable for general purpose applications. Crystallization initiators provide fast molding cycles through rapid melt set-up. Nylene NX4569 has excellent melt stability and good melt strength. NX4569 has excellent grease resistance, toughness, and resistance to abrasion. Optimum processing conditions should provide a melt temperature of 480 - 500ºF at the nozzle.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Water Absorption 1.8 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 83.0 MPaASTM D638
Elongation at Break 70 %ASTM D638
Flexural Yield Strength 103 MPaASTM D790
Izod Impact, Notched 0.400 J/cmASTM D256
 
Processing PropertiesOriginal ValueComments
Processing Temperature 249 - 260 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nylene® PA6 Glass/Mineral Filled 7115 HS Nylon 6
NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Ensinger ENSILON® 6/6 GF30 Extruded Nylon 6/6, 30% glass-fiber-reinforced (PA66)
Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon

PN6C5H / 54251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.