MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chesterton 610 Plus Synthetic Lubricating Fluid
Categories: Fluid; Lubricant

Material Notes:
  • Wide temperature range
  • Biodegradable
  • 100% synthetic
  • No residue or varnish buildup
  • Low evaporation rate
  • High flash point

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/cc
Viscosity Measurement >= 130>= 130Index; ASTM D2270, ISO 2909
Kinematic Viscosity at 40°C (104°F) 61 - 75 cSt61 - 75 cStASTM D445, DIN 51 561
Kinematic Viscosity at 100°C (212°F) 9.0 - 11 cSt9.0 - 11 cStASTM D445, DIN 51 561
Evaporation Loss 1.9 %
@Temperature 204 °C,
Time 79200 sec
1.9 %
@Temperature 399 °F,
Time 22.0 hour
ASTM D972
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.116 W/m-K
@Temperature 260 °C
0.805 BTU-in/hr-ft²-°F
@Temperature 500 °F
 0.135 W/m-K
@Temperature 10.0 °C
0.937 BTU-in/hr-ft²-°F
@Temperature 50.0 °F
Maximum Service Temperature, Air 270 °C518 °F
Minimum Service Temperature, Air -25.0 °C-13.0 °F
Pour Point -45.0 °C-49.0 °FASTM D97, ISO 3016
Flash Point 310 °C590 °FCOC; ASTM D92, ISO 2592
 
Descriptive Properties
AppearanceAmber Liquid
Fire Point330°CASTM D92, ISO 2592

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS078e / 239861

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.