MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Chemlon® 133 GH Nylon 66, 33% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Availability: Asia Pacific; Europe; North America

Fillers/Reinforcement: Glass Fiber, 33% Filler by Weight

Additive: Heat Stabilizer; Lubricant

Features: Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated

Automotive Specifications: 3M 11-0003-5762-1; CHRYSLER MS-DB-41 CPN1900 Color: BK001 Black; CHRYSLER MS-DB-41 CPN2224 Color: Non-matched Color; FORD ESB-M4D133-A; FORD ESB-M4D89-A; FORD WSK-M4D663-A; GM GMP.PA66.013 Color: Natural; GM GMW3038P-PA66-GF35H

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ASTM D792
Water Absorption 0.90 %
@Time 86400 sec
0.90 %
@Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage, Flow 0.0015 - 0.0040 cm/cm0.0015 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 176 MPa25500 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Elongation at Yield 3.0 %3.0 %ASTM D638
Flexural Strength 276 MPa40000 psiASTM D790
Flexural Modulus 8.62 GPa1250 ksiASTM D790
Izod Impact, Notched 1.07 J/cm2.00 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 16.1 kV/mm
@Thickness 3.00 mm
410 kV/in
@Thickness 0.118 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 50.4 µm/m-°C28.0 µin/in-°FASTM D969
Deflection Temperature at 1.8 MPa (264 psi) 249 °C480 °FUnannealed; ASTM D648
UL RTI, Electrical  95.0 °C
@Thickness 0.762 mm
203 °F
@Thickness 0.0300 in
UL 746
 110 °C
@Thickness 1.52 mm
230 °F
@Thickness 0.0600 in
UL 746
 110 °C
@Thickness 3.05 mm
230 °F
@Thickness 0.120 in
UL 746
UL RTI, Mechanical with Impact  95.0 °C
@Thickness 0.762 mm
203 °F
@Thickness 0.0300 in
UL 746
 110 °C
@Thickness 1.52 mm
230 °F
@Thickness 0.0600 in
UL 746
 110 °C
@Thickness 3.05 mm
230 °F
@Thickness 0.120 in
UL 746
UL RTI, Mechanical without Impact  130 °C
@Thickness 0.762 mm
266 °F
@Thickness 0.0300 in
UL 746
 130 °C
@Thickness 1.52 mm
266 °F
@Thickness 0.0600 in
UL 746
 130 °C
@Thickness 3.05 mm
266 °F
@Thickness 0.120 in
UL 746
Flammability, UL94 HB
@Thickness 0.762 mm
HB
@Thickness 0.0300 in
Oxygen Index 25 %25 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 246 - 257 °C475 - 495 °F
Middle Barrel Temperature 263 - 274 °C505 - 525 °F
Front Barrel Temperature 268 - 282 °C515 - 540 °F
Nozzle Temperature 268 - 282 °C515 - 540 °F
Melt Temperature 257 °C495 °F
 263 - 282 °C505 - 540 °F
Mold Temperature 60.0 - 93.3 °C140 - 200 °F
Drying Temperature 79.4 °C175 °F
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Screw Speed 60 - 120 rpm60 - 120 rpm
 
Descriptive Properties
AppearanceBlack
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0468 / 236959

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.