MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Nucrel® 903 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Film Grade

Material Notes: 9 wt% Methacrylic Acid.

Nucrel® 0903 is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.

Features/Benefits vs. Nucrel® 0902HC: Higher melt flow index provides easier extrusion, higher extrusion rates, and higher flow during heat sealing. The result is fewer leakers.

Typical Applications: Meat, poultry, seafood, and cheese packaging; Cereal liners; Medical/pharmaceutical packaging; Powdered/granular food and non-food pouches; Carded display/skin packaging films; Edible oil, motor oil, and other liquid product pouches; Snack structures; Coextrusions with nylon or in other film structures as a heat seal or tie layer.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 %50 µm (2 mil) film; ASTM D882
Film Elongation at Break, TD 500 %50 µm (2 mil) film; ASTM D882
Secant Modulus, MD 0.103 GPa50 µm (2 mil) film; ASTM D882
Secant Modulus, TD 0.110 GPa50 µm (2 mil) film; ASTM D882
Impact 24J/mm Spencer Impact; ASTM D3420
Elmendorf Tear Strength, MD 140 g/mil50 µm (2 mil) film; ASTM D1922
Elmendorf Tear Strength, TD 190 g/mil50 µm (2 mil) film; ASTM D1922
Dart Drop Test 5.90 g
Seal Strength 1400 g/25 mmseal bar 140°C.
Hot Tack Strength 1800 g/25 mmseal bar 105°C; Packforsk method.
Film Tensile Strength at Break, MD 31.7 MPa50 µm (2 mil) film; ASTM D882
Film Tensile Strength at Break, TD 35.2 MPa50 µm (2 mil) film; ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 83.0 °CFreezing Point via DSC/ASTM D3418
 101 °CUpon Melting via DSC/ASTM D3418
Vicat Softening Point 81.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 3.5 %ASTM D1003
Gloss 60 %20°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 191 °CTypical Die Temp.
Melt Temperature 190 - 218 °Cblown film equipment

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Dow Nucrel® 0609HSA Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
Dow Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating
Dow Nucrel® AE High Performance Adhesive and Sealant Resin
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer

PDUPJ6 / 33640

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.