MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT Group Moldmaster Cat Red Condensation Fast Cure, Moldmaking Catalyst for QM 2125, QM 2128 and QM 2225
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: Moldmaster Cat Red is a two-component, room temperature, fast, condensation cure catalyst for QM 2125, QM 2128 and QM 2225. The cured rubber has excellent mechanical properties and good shelf-life stability. There are a variety of catalysts which allow for variable cure speeds, offered with the Moldmaster base series. Styrene resistant catalysts are also available.

Key Features:

  • Quick tack-free time
  • Fast demold time
  • Minimal impact on cured physical properties
Main Applications:
  • Molds for polyester, polyurethane and epoxy resin castings
  • Molds for large and small statues
  • Molds for technical articles and prototypes
  • Molds for furniture and picture frame replication
  • Molds for GFRC pre-cast

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccUncatalyzed
Viscosity 100 cP100 cPUncatalyzed
 
Processing PropertiesMetricEnglishComments
Cure Time 240 - 360 min4.00 - 6.00 hourDemold time, Catalyzed
Tack-Free Time 120 - 240 min2.00 - 4.00 hourCatalyzed
Pot Life 30.0 min30.0 minCatalyzed
 
Descriptive Properties
ColorLight RedCatalyzed
 RedUncatalyzed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PACC2067 / 199455

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.