MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Saint-Gobain Norton® OmniFlex™ R11 High Performance Fluoroelastomer Seal  (discontinued **)
Categories: Polymer

Material Notes: OmniFlex™ is a fluoroelastomer material with performance equivalent to perfluoroelastomer materials in chemical resistance and inertness yet with a softer durometer and improved compression set. OmniFlex™ has outstanding temperature performance of -70°F (-57°C) which outperforms perfluoroelastomer materials.

R11 Features/Benefits: Good chemical resistance and inertness, Good compression set, Excellent low temperature performance.

SOLVENT COMPATIBILITY: Toluene, Gasoline, Methyl Alcohol, Acetone, Methyl Tertiary Butyl Ether. CHEMICAL COMPATIBILITY: Hydrochloric Acid, Sulfuric Acid, Nitric Acid, Sodium Hydroxide, Butylamine.

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 g/cc1.85 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7070ASTM D2240
Tensile Strength, Yield 5.96 MPa865 psiASTM D412
Elongation at Break 450 %450 %ASTM D412
50% Modulus 4.50 MPa
@Strain 50 %
4.50 MPa
@Strain 50 %
ASTM D412
100% Modulus 2.55 MPa
@Strain 100 %
370 psi
@Strain 100 %
ASTM D412
Compression Set 12 %
@Temperature 200 °C
12 %
@Temperature 392 °F
Constant Deflection, 70 hrs.; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 218 °C425 °F
Minimum Service Temperature, Air -56.7 °C-70.0 °F
 -50.0 °C-58.0 °FRetraction; ASTM D1329
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQZ209 / 68723

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.