  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyram PlusTek PB901 Nylon 6, Extruded cable coating
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Polyamide 6 for very thin electrical extruded cable coating

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDIN 53479
Water Absorption 1.9 %DIN 53495
Linear Mold Shrinkage 0.010 - 0.012 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 85.0 MPaASTM-D638
Elongation at Break 100 %ASTM-D638
Flexural Strength 110 MPaASTM D790
Flexural Modulus 2.50 GPaASTM-D790
Izod Impact, Notched 0.300 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmDIN 53482
Surface Resistance 1.00e+15 ohmDIN 53482
Dielectric Constant 3.5
@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 100 kV/mmVDE 0303/4
 
Thermal PropertiesOriginal ValueComments
Melting Point 218 °C
Maximum Service Temperature, Air 80.0 °CContinuous Use
 150 °CShort peaks operation
Deflection Temperature at 0.46 MPa (66 psi) 160 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CDIN 53461
Flammability, UL94 V-2
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYRA201 / 57463

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.