MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sylvania SD254 Tungsten & Chrome Based Thermal Spray Powder
Categories: Ceramic; Carbide; Metal; Nonferrous Metal; Tungsten Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: General Description

SD254 is an ultra-fine tungsten carbide-cobalt plasma-spray powder. The major constituent is W2C. WC as well as Co-W-C compounds are present. The material is too fine to exhibit a Hall flow.

Applications

  • Any application which requires a thin (less than 0.003 inch), smooth, wear-resistant coating, such as low pressure bearing surfaces. As-sprayed coatings are dense and smooth and require little, if any, final finishing.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 3.36 - 3.97 g/cc0.121 - 0.143 lb/in³
Particle Size <= 10 µm<= 10 µm90 wt% min; ASTM B822
 <= 44 µm<= 44 µm100 wt% min; ASTM B822
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.8 - 4.5 %3.8 - 4.5 %
Cobalt, Co 10 - 12 %10 - 12 %
Iron, Fe <= 2.0 %<= 2.0 %
Tungsten, W 81.5 - 86.2 %81.5 - 86.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sylvania SX276 Molybdenum Thermal Spray Powder
Sylvania SX158 Tungsten & Chrome Based Thermal Spray Powder
Aluminum 6061-T6; 6061-T651

CSYLV14 / 2313

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.