MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Sika SikaHyflex® 407 EverFlash Universal Universal Flashing and Weather Barrier Sealant
Categories: Polymer; Thermoset

Material Notes: SikaHyflex-407 EverFlash Universal is a one-component, hybrid technology, non-sag, flexible, flashing and weather barrier sealant designed for primerless adhesion to the most challenging substrates found in the building envelope such as peel & stick window and flashing membranes. Meets ASTM C920, Type S, Grade NS, Class 12.5, use NT, G, A, O, M.

Where to Use:

  • Peel & stick window flashing and wraps.
  • Nonwoven spunbound window flashing and wraps.
  • Polyethylene wraps and surfaces, polypropylene surfaces and common polyolefins.
  • PVC, steel, metal, aluminum and glass.
  • All connection details specified for the building envelope to achieve a weather tight building.
  • Between flanged windows and weather barriers.
  • Termination and transition seals where flashing meets the building envelope.
  • Window and door perimeters where movement is applicable.
  • Connections between the building envelope wrap and roofing systems.
  • Asphaltic/bituminous surfaces that would normally bleed with polyurethane sealants.
  • Sealing around penetrations in weather/air barrier and flashing materials.
  • Self adhered air and vapor barrier field-cut edges, T-joints, reverse laps and terminations.
Advantages:
  • Unprimed adhesion to challenging, low surface tension surfaces such as polyethylene, polypropylene and polyolefins.
  • Compatible with bituminous and asphalt based materials – will not cause bleeding.
  • Excellent long term UV and weatherability.
  • Can be painted over with most acrylic coatings.

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30ASTM D412
Tensile Strength 200 psiASTM D412
Elongation at Break 250 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 170 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Tack-Free Time 30.0 - 90.0 min
Shelf Life 12.0 Month
@Temperature 4.00 - 35.0 °C
in original unopened cartridge
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSIKA943 / 209850

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.