MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

3M 9472FL Adhesive Transfer Tape with 300LSE Adhesive
Categories: Polymer; Adhesive

Material Notes: Features:
  • Clear Polyester (PET)
  • Quick flowing acrylic adhesive speeds lamination process
  • Excellent initial adhesion, especially to LSE (low surface energy) plastics
  • Bonds graphics to powder coatings, LSE plastics and oily metals
  • Use on textured plastics, fabrics and coated papers
  • Moisture-stable liner is rotary die-cutable

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 50.8 microns2.00 milLiner
 127 microns5.00 milAdhesive
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 1.118 kN/m6.375 pliABS, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 1.1942 kN/m6.8125 pliStainless Steel, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 1.2600 kN/m7.1875 pliPolypropylene, 90° peel, 2 mil aluminum backing, 15 min RT; ASTM D3330
 1.40 kN/m8.00 pliABS, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 1.49 kN/m8.50 pliPolypropylene, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 1.53 kN/m8.75 pliStainless Steel, 90° peel, 2 mil aluminum backing, 72 hr RT; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 93.0 °C199 °FLong term
 148 °C298 °FShort term
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive
3M 9471 Adhesive Transfer Tapes with Adhesive 300
3M 9462P Adhesive Transfer Tapes with Adhesive 100

PMM33219 / 167966

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.