MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® DP 2-2240/15 H2.0 901510 Nylon 66 (PA66), 15% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Glass Fiber Filled

Material Notes: PA 66, 15% glass fibers, branched, high viscosity and outstanding melt strength, heat-stabilized, good hydrolysis resistance

Extruded profiles and blow molded parts, profiles, especially window insulation profiles, hollow parts and pipes for the automotive cooling circuit

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ISO 1183
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 290 °C
5.0 g/10 min
@Load 11.0 lb,
Temperature 554 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.0 MPa10900 psi5 mm/min; ISO 527-1,-2
Elongation at Break 15 %15 %5 mm/min; ISO 527-1,-2
Tensile Modulus 3.50 GPa508 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 110 MPa16000 psi2 mm/min; ISO 178-A
Flexural Yield Strength 80.0 MPa
@Strain 3.5 %
11600 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 2.70 GPa392 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 8.0 %8.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO) 75.0 kJ/m²
@Temperature 23.0 °C
35.7 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched  5.00 J/cm²
@Temperature -30.0 °C
23.8 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
 9.00 J/cm²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
Charpy Impact, Notched  <= 1.00 J/cm²
@Temperature -30.0 °C
<= 4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °F10°C/min; ISO 11357-1,-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos ABS NOVODUR® P2T ABS, Injection Grade
Envalior Durethan® DP 2-2240/15 H2.0 901510 Nylon 66 (PA66), 15% Glass Fiber Reinforced, Dry
Ravago Manufacturing Americas Hylon N1035HHR Nylon 66, DAM
Envalior Durethan® DP 2325 H3.0 000000 Nylon 66 (PA66), Conditioned
Envalior Durethan® A 30 H2.0 901510 Nylon 66

PLANW9505 / 208332

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.