Product Description: Terratek® GDH-B1FA is a unique elastomeric bioplastic with a diverse range of potential applications. The bioplastic is verified to meet U.S. (ASTM D6400-04) and E.U. (EN13432) standards for compostability. Applications: This material is suitable for injection molding, profile extrusion, sheet extrusion, blow molding, and blown film. Information provided by Green Dot Bioplastics |