MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Westlake Plastics Tempalux® 5000 Polyetherimide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, high modulus, and broad chemical resistance. Tempalux stock shapes are inherently flame resistant with low smoke emission. Tempalux stock shapes display property retention and resistance to environmental stress cracking when exposed to a wide variety of chemicals. The standard color of Tempalux stock shapes is light amber.

Applications Include:

  • Medical instrument trays
  • Burn-in test sockets
  • Aircraft / Aerospace interiors
  • Connectors
  • Automotive components
  • Valves, electrical fittings
  • Food service (ovenable)
  • Flex Circuits

Advantages of Tempalux 5000:

  • Inherent flame resistance
  • Extremely low NBS smoke evolution
  • Superior limiting oxygen index
  • Exceptional flexural and tensile strength
  • Broad chemical resistance
  • UV stable - inherently
  • FDA Compliant

Information provided by Westlake Plastics Company.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/in
@Thickness 3.20 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 in/in
@Thickness 3.20 mm
ASTM D955
Melt Flow 12.5 g/10 min
@Load 6.60 kg,
Temperature 367 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14000 psiASTM D638
Tensile Strength, Yield 14000 psiASTM D638
Elongation at Break 25 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Tensile Modulus 510 ksiASTM D638
Flexural Strength 23100 psi1.97" span; ASTM D790
Flexural Yield Strength 22500 psi3.94" span; ASTM D790
Flexural Modulus 460 ksi1.97" span; ASTM D790
Izod Impact, Notched 1.30 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 1.39 ft-lb/in
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched NBASTM D256
Dart Drop, Total Energy 25.0 ft-lbInstrumented; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 432 V/milin Oil, 0.126 in; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 µin/in-°F
@Temperature -40.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 28.0 µin/in-°F
@Temperature -40.0 - 150 °C
ASTM E831
Thermal Conductivity 1.50 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 459 °F
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 423 °F
@Thickness 3.20 mm
unannealed; ASTM D648
 446 °F
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 468 °F
@Load 5.10 kg
Rate B; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %ASTM D1746
Transmission, Visible 58 %Transmittance; ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Tempalux® CN-F Polyetherimide (conductive)
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin
Mitsubishi Chemical Advanced Materials Semitron™ MP-370 Polyphenylsulfone
Covestro Makroblend® UT-640 G Polycarbonate + Polyester Blend
Covestro Apec® DP 1-9389 Polycarbonate

PWEST994 / 131204

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.