Metal Series: fast bonding and high viscosity. Cyanoacrylates are not really made to bond metal to metal. But when it comes to combinations with rubber or plastic, these products can be very suitable. Due to its high viscosity CB 1699 can fill smaller gaps.Information provided by H.B. Fuller Company |