MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LATI Latiblend 7587 E61-V0 PBT/PC, Flame Retardant
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Blend based on Polybutylene Terephthalate (PBT) / Polycarbonate (PC). Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. High impact resistance.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
Linear Mold Shrinkage, Flow 0.012 - 0.015 cm/cm0.012 - 0.015 in/in
Linear Mold Shrinkage, Transverse 0.011 - 0.014 cm/cm0.011 - 0.014 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  20.0 MPa
@Temperature 60.0 °C
2900 psi
@Temperature 140 °F
 30.0 MPa
@Temperature 23.0 °C
4350 psi
@Temperature 73.4 °F
Elongation at Break  20 %
@Temperature 23.0 °C
20 %
@Temperature 73.4 °F
 75 %
@Temperature 60.0 °C
75 %
@Temperature 140 °F
 >= 100 %
@Temperature 90.0 °C
>= 100 %
@Temperature 194 °F
 >= 100 %
@Temperature 120 °C
>= 100 %
@Temperature 248 °F
Elongation at Yield  5.0 %
@Temperature 23.0 °C
5.0 %
@Temperature 73.4 °F
 >= 10 %
@Temperature 60.0 °C
>= 10 %
@Temperature 140 °F
 >= 10 %
@Temperature 90.0 °C
>= 10 %
@Temperature 194 °F
 >= 10 %
@Temperature 120 °C
>= 10 %
@Temperature 248 °F
Tensile Modulus  1.00 GPa
@Temperature 120 °C
145 ksi
@Temperature 248 °F
 1.20 GPa
@Temperature 90.0 °C
174 ksi
@Temperature 194 °F
 1.40 GPa
@Temperature 60.0 °C
203 ksi
@Temperature 140 °F
 1.90 GPa
@Temperature 23.0 °C
276 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched NBNB
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 200 V200 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °F
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °F
Vicat Softening Point 120 °C
@Load 5.00 kg
248 °F
@Load 11.0 lb
Flammability, UL94  V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 V-0
@Thickness 15.0 mm
V-0
@Thickness 0.591 in
Oxygen Index 29 %29 %
Glow Wire Test  960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
GWFI/GWT
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 120 - 130 °C
@Time 10800 sec
248 - 266 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kingfa PC-S609 Toughened PC

PLATH9791 / 177487

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.