MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay Chemicals Liquid Caustic Soda (Sodium Hydroxide, NaOH) 20-29% Aqueous Solution
Categories: Fluid

Material Notes: EINECS Number: 215-185-5/CAS Number: 1310-73-2

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/cc
@Temperature 100 °C
Concentration, 200 g NaOH/kg
 1.176 g/cc
@Temperature 90.0 °C
Concentration, 200 g NaOH/kg
 1.183 g/cc
@Temperature 80.0 °C
Concentration, 200 g NaOH/kg
 1.189 g/cc
@Temperature 70.0 °C
Concentration, 200 g NaOH/kg
 1.196 g/cc
@Temperature 60.0 °C
Concentration, 200 g NaOH/kg
 1.202 g/cc
@Temperature 50.0 °C
Concentration, 200 g NaOH/kg
 1.207 g/cc
@Temperature 40.0 °C
Concentration, 200 g NaOH/kg
 1.213 g/cc
@Temperature 30.0 °C
Concentration, 200 g NaOH/kg
 1.219 g/cc
@Temperature 20.0 °C
Concentration, 200 g NaOH/kg
 1.224 g/cc
@Temperature 10.0 °C
Concentration, 200 g NaOH/kg
 1.229 g/cc
@Temperature 0.000 °C
Concentration, 200 g NaOH/kg
Viscosity 0.68 cP
@Temperature 100 °C
Concentration 0.20 kg NaOH/kg
 0.84 cP
@Temperature 90.0 °C
Concentration 0.20 kg NaOH/kg
 0.94 cP
@Temperature 100 °C
Concentration 0.25 kg NaOH/kg
 1.03 cP
@Temperature 80.0 °C
Concentration 0.20 kg NaOH/kg
 1.16 cP
@Temperature 90.0 °C
Concentration 0.25 kg NaOH/kg
 1.26 cP
@Temperature 70.0 °C
Concentration 0.20 kg NaOH/kg
 1.44 cP
@Temperature 80.0 °C
Concentration 0.25 kg NaOH/kg
 1.57 cP
@Temperature 60.0 °C
Concentration 0.20 kg NaOH/kg
 1.8 cP
@Temperature 70.0 °C
Concentration 0.25 kg NaOH/kg
 1.93 cP
@Temperature 50.0 °C
Concentration 0.20 kg NaOH/kg
 2.26 cP
@Temperature 60.0 °C
Concentration 0.25 kg NaOH/kg
 2.43 cP
@Temperature 40.0 °C
Concentration 0.20 kg NaOH/kg
 2.87 cP
@Temperature 50.0 °C
Concentration 0.25 kg NaOH/kg
 3.17 cP
@Temperature 30.0 °C
Concentration 0.20 kg NaOH/kg
 3.76 cP
@Temperature 40.0 °C
Concentration 0.25 kg NaOH/kg
 4.43 cP
@Temperature 20.0 °C
Concentration 0.20 kg NaOH/kg
 5.15 cP
@Temperature 30.0 °C
Concentration 0.25 kg NaOH/kg
 7.45 cP
@Temperature 20.0 °C
Concentration 0.25 kg NaOH/kg
Molecular Weight 40.01 g/molNaOH
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 3.49 J/g-°C
@Temperature 10.0 °C
Concentration 0.28 kg NaOH/kg
 3.50 J/g-°C
@Temperature 0.000 °C
Concentration 0.22 kg NaOH/kg
 3.51 J/g-°C
@Temperature 10.0 °C
Concentration 0.26 kg NaOH/kg
 3.52 J/g-°C
@Temperature 0.000 °C
Concentration 0.20 kg NaOH/kg
 3.53 J/g-°C
@Temperature 10.0 °C
Concentration 0.24 kg NaOH/kg
 3.62 J/g-°C
@Temperature 50.0 °C
Concentration 0.28 kg NaOH/kg
 3.63 J/g-°C
@Temperature 50.0 °C
Concentration 0.26 kg NaOH/kg
 3.65 J/g-°C
@Temperature 50.0 °C
Concentration 0.24 kg NaOH/kg
 3.65 J/g-°C
@Temperature 100 °C
Concentration 0.28 kg NaOH/kg
 3.66 J/g-°C
@Temperature 50.0 °C
Concentration 0.22 kg NaOH/kg
 3.67 J/g-°C
@Temperature 100 °C
Concentration 0.26 kg NaOH/kg
 3.68 J/g-°C
@Temperature 100 °C
Concentration 0.24 kg NaOH/kg
 3.68 J/g-°C
@Temperature 50.0 °C
Concentration 0.20 kg NaOH/kg
 3.69 J/g-°C
@Temperature 100 °C
Concentration 0.22 kg NaOH/kg
 3.71 J/g-°C
@Temperature 100 °C
Concentration 0.20 kg NaOH/kg
Boiling Point 108 °CConcentration, 0.20 kg NaOH/kg
 112.5 °CConcentration, 0.25 kg NaOH/kg
 
Descriptive Properties
Colorcolorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay Chemicals Liquid Caustic Soda (Sodium Hydroxide, NaOH) 70-79% Aqueous Solution
Ovako 12NiCr14-6* 245S Steel, Soft annealing

WSOLV123g / 234810

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.