MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

PolyMirae Moplen EP648N Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Moplen EP648N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP648N is a high gloss block copolymer particularly suitable for injection molding of parts of electrical appliances, containers. Moplen EP648N meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520.

Features: Optimized balance of stiffness and toughness; High gloss; High stiffness; Heat resistance; Scratch resistance;

Applications: Parts of electrical appliances; Containers

Information provided by PolyMirae Company Ltd.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 9.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
9.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Tensile Strength, Yield 34.3 MPa4980 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus 1.81 GPa263 ksiASTM D790
Izod Impact, Notched 0.981 J/cm1.84 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C266 °FASTM D648
Vicat Softening Point 153 °C307 °FASTM D1525
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PolyMirae Moplen HP620M CPP Film Grade Polypropylene
Aclo Accucomp Polypropylene HPO306L Homopolymer
Aclo Accutech Polypropylene CP0437T40V Copolymer Talc Reinforced
Aclo Accutech Polypropylene CP0435G20HIV Copolymer Glass Reinforced High Impact
Aclo Accutech Polypropylene CP0409HUUVV Copolymer UV Stabilized

PMIRAE24 / 53136

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.